小方坯、板坯连铸机拉矫辊、支承辊主要采用25CrMo435CrMo42CeMo60CrMoV60CrNiMo、及Cr5Cr8等合金工具钢制造,我公司研究生产的复合材料小方坯、板坯拉矫辊比整体合金钢辊提高使用寿命5-8倍,达到进口复合辊的寿命,且辊面可多次修复使用。冷轧工作辊,支承辊、钢板矫直辊淬硬层有效深度达单面25毫米以上。

Small billet, slab continuous caster roll and backup roll mainly adopts 25 crmo4, 35 crmo, cemo, 60 crmov, 60 crnimo and 42 Cr5, Cr8 alloy tool steel, such as manufacturing, our company research and production of composite material small billet, slab pull roller than the overall alloy steel roller correction to improve the service life of 5-8 times, to import the life of the composite roll, and roll surface can be used many times to repair. Cold rolled work roll and backup roll, plate straightening roll the effective depth of hardening layer of single side more than 25 mm.